A Ni-based alloy member has resistance against grain boundary fracture,
fatigue strength, and oxidation resistance at temperatures near
1000.degree. C. or higher. The Ni-based alloy member includes a
non-repaired region made of a Ni-based alloy base and a region repaired
by welding, which is formed on the non-repaired region and which is made
of a buildup-welded layer, the buildup-welded layer being made of a
Ni-based alloy containing, by weight, 15% or less of Co, 18-22% of Cr,
0.8-2.0% of Al, 5.0% or less of Ta, 0.5% or less of Mo, 0.5% or less of
Ti, 13-18% of W, 0.05-0.13% of C, 0.06% or less of Zr, 0.015% or less of
B, 0.4-1.2% of Mn, and 0.1-0.3% of Si, the balance of the alloy being
preferably essentially made of Ni.