To provide a thermoplastic elastomer composition which is excellent in
light resistance and flexibility and has high tear strength. [MEANS FOR
SOLVING PROBLEMS] A thermoplastic elastomer composition comprising 100
parts by mass of acrylic multi-layer polymer particles (A) which each
comprise at least two layers, i.e., at least one inner rubber layer (I)
and at least one outermost thermoplastic resin layer (II), 5 to 300 parts
by mass of an ethylene/vinyl ester copolymer (B), and 0.5 to 150 parts by
mass of a graft copolymer (C) composed of an ethylene/vinyl ester
copolymer backbone and a graft bonded to the backbone which consists of
units derived from a monomer having a polarity higher than that of the
backbone.