A solid state reaction method for the production of tetrabasic lead sulfate includes the steps of mixing a stoichiometric mixture of 5PbO and (NH.sub.4).sub.2SO.sub.4 and heating the stoichiometric mixture of 5PbO and (NH.sub.4).sub.2SO.sub.4 at a temperature between 500 and 700.degree. C. for 3 to 8 hours. The method also includes the steps of deagglomerating and sieving resulting tetrabasic lead sulfate.

 