Multimodal polyethylenes possessing a density from 0.940 to 0.965 g/cm.sup.3, and an I.sub.21 from 4 to 20 dg/min, and comprising a low molecular weight ethylene copolymer having a weight average molecular weight from 5,000 amu to 50,000 amu; and a high molecular weight ethylene copolymer having a weight average molecular weight from 60,000 amu to 800,000 amu, both components having a desirable balance of short chain branching making the multimodal polyethylene suitable for films, pipes, rotomolding applications and blow molding applications.

 