New methods for activating chromium catalysts for polymerization processes
decrease the amount of time required for activation and increase catalyst
activity. Rapid heating to a first temperature is followed by a first
hold period before heating to a higher second temperature and maintaining
the second temperature for a second hold period. In one aspect, the
overall activation process takes less than 10 hours.