A method of recycling commingled plastics waste containing min. 30 wt. %
of polyolefins to a tough thermoplastic material, based on the
compatibilization of the polymer components of commingled plastics waste
with an admixture of 2-15 wt. % of an ethylene--propylene copolymer or a
styrene--butadiene block copolymer or a combination of an
ethylene--propylene copolymer and a styrene--butadiene copolymer in any
weight ratio, together with 0.1-2.5 wt. % of a secondary aromatic amine
and by subsequent blend processing in the melt.