Nanostructured layers with 10 nm to 50 nm pores spaced 10-50 nm apart, a
method for making such nanostructured layers, optoelectronic devices
having such nanostructured layers and uses for such nanostructured layers
are disclosed. The nanostructured layer can be formed using precursor
sol, which generally includes one or more covalent metal complexes, one
or more surfactants, a solvent, one or more optional condensation
inhibitors, and (optionally) water. Evaporating the solvent from the
precursor sol forms a surfactant-templated film. Covalently crosslinking
the surfactant-templated film forms a nanostructured porous layer. Pore
size is controlled, e.g., by appropriate solvent concentration, choice of
surfactant, use of chelating agents, use of swelling agents or
combinations of these.