A cellulose acylate film that has a crystallization index expressed by
expression (A) as defined in the specification of from 0.70 to 1.02 and a
modulus of elasticity in every arbitrary direction of an in-plane of the
cellulose acylate film of from 3,800 MPa to 6,000 MPa; a manufacturing
method of a cellulose acylate film comprising: casting a dope on a
support; drying the dope on the support, so as to form a film; peeling
the film from the support; and subjecting the film to a stretching
treatment, wherein a crystallization index expressed by expression (A) of
the film after peeling and before stretching is from 0.70 to 1.00; an
optically compensatory sheet comprising the cellulose acylate film; and a
polarizing plate and a liquid crystal display device using the optically
compensatory sheet.