The invention relates to a method for producing a high-molecular
polycondensate from a solidified polycondensate prepolymer by solid phase
polycondensation. According to said method, the polycondensation cleavage
products of the solid phase polycondensation reaction are extracted from
the product by means of a process gas, and the process gas is then
cleaned of the polycondensation cleavage products and essentially
recycled. According to the invention, the specific energy input is less
than 120 kWh/t, preferably less than 110 kWh/t and especially between 70
and 100 kWh/t. The invention also relates to an installation for
producing a high-molecular polycondensate, said installation comprising a
heating appliance (1), followed by a crystallisation appliance (2), a
reaction appliance (4), and a cooling appliance (5). A gas outlet (5d) of
the cooling appliance (5) is connected to a gas inlet (1c) of the heating
appliance (1), a gas outlet (4d) of the reaction appliance (4) is
connected to a gas inlet (6c) in a gas cleaning system (6), and a gas
outlet (6d) of the gas cleaning system (6) is connected to a gas inlet
(4c) of the reaction appliance (4).