A process is described for production of a biaxially oriented film which comprises at one crystallizable thermoplastic as main constituent and comprises at least 500 ppm, based on the weight of thermoplastic, of a pigment. The production process uses at least 20% by weight, based on the weight of the film, of recycled material of the same type whose molecular weight has been increased by condensation processes.

 