According to one embodiment, a method for forming a transparent ceramic
preform includes forming a suspension of oxide particles in a solvent,
adding the suspension to a mold of a desired shape, and uniformly curing
the suspension in the mold for forming a preform. The suspension includes
a dispersant but does not include a gelling agent. In another embodiment,
a method includes creating a mixture without a gelling agent, the mixture
including: inorganic particles, a solvent, and a dispersant. The
inorganic particles have a mean diameter of less than about 2000 nm. The
method also includes agitating the mixture, adding the mixture to a mold,
and curing the mixture in the mold at a temperature of less than about
80.degree. C. for forming a preform. Other methods for forming a
transparent ceramic preform are also described according to several
embodiments.