A method of forming a gypsum-based panel product including the steps of:
mixing calcined gypsum, water, a foaming agent and a core strengthening
agent to form a foamed slurry; depositing the slurry; shaping the slurry
to form a board having a core and core surfaces, optionally sandwiched
between sheets of liner; and allowing the core to set, and drying the
board, wherein the strengthening agent is dextrin, used in an amount not
less than 0.1% by weight, based on the amount of calcined gypsum, so
that, after drying, there is provided a strengthening dispersion of
dextrin throughout the core. Less than 5% dextrin in preferred.