In order to create titanium components with a titanium composite insert, a
method is provided whereby an initial pre form 1 has a groove 2 formed in
it. An encapsulating member 4 is then provided about the groove 2 in
order to create a cavity 5 which is filled with titanium alloy powder 6.
This titanium alloy powder 6 is densified and then accurately machined in
order to create a groove insert form 7 which can accommodate a titanium
composite material pre form insert 8 and further titanium alloy powder 9
such that through a high temperature isostatic pressing (HIP) process,
the insert 8 is embedded. The original component form 1 can then be
machined in order to create the final component elements such as
aerofoils 13.