Disclosed is a method for manufacturing a multimode optical fiber for high data rate LAN using MCVD, which includes a deposition process for forming a clad layer and a core layer, doped with an additive for controlling a refractive index, on an inner wall of a quartz tube by injecting a deposition gas into the quartz tube and applying heat to outside of the quartz tube; and a collapse process, which is repeatedly conducted N times, for filling up a gap in the quartz tube by applying heat of a temperature over a deposition temperature to the quartz tube after the core layer is completely deposited. In the method, together with an N-1.sup.th collapse process, an etching process of injecting a reaction gas for etching into the quartz tube is conducted in order to eliminate a portion of which refractive index is transformed due to evaporation of the additive.

 