The specification describes a method for the manufacture of fluoride glass
optical fibers which are covered with a protective coating of phosphate
glass. The coating is produced by dipping the fluoride glass preform in a
phosphate glass melt prior to drawing the optical fiber. The fluoride
glass is ZBLAN. The phosphate glass has a glass transition temperature
below 200.degree. C., which allows the dipping step to be carried out at a
relatively low temperature where the preform temperature is maintained
well below the crystallization temperature of the fluoride glass, and also
where the viscosity of the fluoride glass preform is substantially higher
than the viscosity of the phosphate glass coating material.