A process for producing a polyethylene resin having a monomodal molecular
weight distribution in a single polymerisation reactor using a
chromium-based catalyst system, by copolymerising ethylene and an
alpha-olefinic-comonomer having from 3 to 8 carbon atoms, the polyethylene
resin comprising a blend of a higher molecular weight fraction polymerised
by a first chromium-based catalyst of the system and a lower molecular
weight fraction polymerised by a second chromium-based catalyst of the
system, wherein the comonomer incorporation in the higher molecular weight
fraction is greater than the comonomer incorporation in the lower
molecular weight fraction is greater than the comonomer incorporation in
the lower molecular weight fraction whereby the higher and lower molecular
weight fractions differ in density by from 0.01 to 0.03 g/cc.
Un procédé pour produire une résine de polyéthylène ayant une distribution monomodal de poids moléculaire dans un réacteur simple de polymérisation en utilisant un système chrome-basé de catalyseur, par copolymerising l'éthylène et un alpha-oléfinique-comonomère ayant de 3 à 8 atomes de carbone, la résine de polyéthylène comportant un mélange d'une plus haute fraction de poids moléculaire polymérisée par un premier catalyseur chrome-basé du système et d'une fraction inférieure de poids moléculaire a polymérisé par un deuxième catalyseur chrome-basé du système, où l'incorporation de comonomère dans la fraction plus haute de poids moléculaire est plus grande que l'incorporation de comonomère dans la fraction inférieure de poids moléculaire est plus grande que l'incorporation de comonomère dans la fraction inférieure de poids moléculaire par lequel les fractions plus hautes et inférieures de poids moléculaire diffèrent dans la densité par de 0.01 à 0.03 g/cc.