A high-Cr steel pipe for line pipes having further improved HAZ toughness and hot workability is provided by limiting the composition to: C: 0.02% or less, Si: 0.5% or less, Mn: 0.2 to 3.0%, Cr: 10.0 to 14.0%, Ni: more than 2.0 to 3.0%, N: 0.02% or less, preferably Nb: 0.3% or less, and the balance being Fe and incidental impurities.

 