This process for the manufacture of norbornene from dicyclopentadiene (DCPD) and ethylene is characterized in that the DCPD is subjected to partial monomerization to CPD by preheating: at a temperature of 140.degree. C. to 240.degree. C.; and under a pressure of 20 to 300 bar abs., before reacting it with the ethylene; with an ethylene/DCPD molar ratio of 1 to 20; at a temperature of 200.degree. C. to 320.degree. C.; under a pressure of 20 to 300 bar abs.; and with a residence time of 1 to 10 minutes, under stable reaction conditions between the DCPD, the CPD and the ethylene.

Este proceso para la fabricación del norbornene del dicyclopentadiene (DCPD) y del etileno se caracteriza en que el DCPD es sujetado al monomerization parcial a CPD por el precalientamiento: en una temperatura de 140.degree. C. a 240.degree. C.; y bajo presión de 20 a 300 ABS de la barra, antes de reaccionarla con el etileno; con un cociente molar de ethylene/DCPD de 1 a 20; en una temperatura de 200.degree. C. a 320.degree. C.; bajo presión de 20 a 300 ABS de la barra; y con un rato de residencia de 1 a 10 minutos, bajo condiciones estables de la reacción entre el DCPD, el CPD y el etileno.

 
Web www.patentalert.com

< Hydrosilylation crosslinking of thermoplastic elastomer

< Resin system

> Rubber composition

> Photoresist monomer, polymer thereof and photoresist composition containing it

~ 00050