The present invention is a rubber modified monovinylidene aromatic polymer
comprising:
a) a monovinylidene aromatic polymer matrix,
b) rubber particles dispersed therein, characterized in that the rubber
particles are produced from a diene rubber having I) a high molecular
weight component and II) a low molecular weight component; the high
molecular weight component having a weight average molecular weight at
least two and one half times greater than the weight average molecular
weight of the low molecular weight component, wherein both components I
and II have a 1,4 cis content of greater than 70 percent and III) the
rubber is grafted with monovinylidene aromatic polymer to the extent that
there is at least 30 percent monovinylidene aromatic polymer present as
grafts on the rubber.
Die anwesende Erfindung ist ein geändertes monovinylidene aromatisches Polymer-Plastik Gummienthalten: A) zerstreute eine monovinylidene aromatische Polymer-Plastik Matrix, B) Gummipartikel darin, dadurch gekennzeichnet, daß die Gummipartikel aus einem Diengummi produziert werden, der I) einen Molekulargewichtbestandteil und II) einen niedermolekularen Gewichtbestandteil hat; der Molekulargewichtbestandteil, der ein Gewichtdurchschnitt Molekulargewicht mindestens zwei und die halben Zeiten eins grösser sind als das Gewichtdurchschnitt Molekulargewicht des niedermolekularen Gewichtbestandteils hat, worin beide Bestandteile I und II einen diesseits Inhalt 1.4 von grösser als 70 Prozent und III) von Gummi haben, wird mit monovinylidene aromatischem Polymer-Plastik verpflanzt, soweit daß es mindestens ein 30 Prozent monovinylidene aromatisches Polymer-Plastik Geschenk als Transplantationen auf dem Gummi gibt.