Recrystallized lead and lead alloy positive electrodes for lead acid
batteries having an increased percentage of special grain boundaries in
the microstructure, preferably to at least 50%, which have been provided
by a process comprising steps of working or straining the lead or lead
alloy, and subsequently annealing the lead or lead alloy. Either a single
cycle of working and annealing can be provided, or a plurality of such
cycles can be provided. The amount of cold work or strain, the
recrystallization time and temperature, and the number of repetitions of
such steps are selected to ensure that a substantial increase in the
population of special grain boundaries is provided in the microstructure,
to improve resistance to creep, intergranular corrosion and intergranular
cracking of the electrodes during battery service, and result in extended
battery life and the opportunity to reduce the size and weight of the
battery.
Рекристаллизованные электроды руководства и сплава руководства положительные для батарей руководства кисловочных имея увеличенный процент специальных границ зерна в микроструктуре, предпочтительн до по крайней мере 50%, которое были обеспечены процессом состоя из шагов работы или напрягать руководство или сплав руководства, и затем обжигая руководство или сплав руководства. Или одиночный цикл работы и обжигать можно обеспечить, или множественность таких циклов можно обеспечить. Количество холодных работы или напряжения, время и температура рекристаллизации, и число повторений таких шагов выбраны для того чтобы обеспечить что обеспечен значительня повышение в населенности специальных границ зерна в микроструктуре, для того чтобы улучшить сопротивление к ползучести, межзерновой корозии и межзерновому трескать электродов во время обслуживания батареи, и результата в выдвинутой жизни батареи и возможности уменьшить размер и вес батареи.