The present invention relates to a composition, particularly useful in
paint. This composition is defined in that it contains, for successive or
simultaneous addition:
an isocyanate which is at least partially masked, having a glass transition
temperature (sometimes denoted by the abbreviation Tg) of at least
20.degree. C., advantageously of at least 40.degree. C., and a degree of
liberation at 120.degree. C. of not more than 5%;
a polyol having the following characteristics:
a glass transition temperature (sometimes denoted by the abbreviation Tg)
which is at least equal to about 40.degree. C., advantageously at least
equal to about 50.degree. C.;
a hydroxyl number at least equal to about 10 mg/g, advantageously at least
equal to about 15 mg/g;
an average molecular mass Mn at least equal to about 1000 g/mol and
advantageously to 2000 g/mol.
La actual invención se relaciona con una composición, particularmente útil en pintura. Esta composición se define en que contiene, para la adición sucesiva o simultánea: un isocianato que se enmascara por lo menos parcialmente, haciendo una temperatura de transición de cristal (denotar a veces por la abreviatura Tg) por lo menos de 20.degree. C., ventajoso por lo menos de 40.degree. C., y un grado de la liberación en 120.degree. C. de no más el que 5%; un polyol que tiene las características siguientes: una temperatura de transición de cristal (denotada a veces por la abreviatura Tg) que es por lo menos igual alrededor a 40.degree. C., ventajoso por lo menos igual alrededor a 50.degree. C.; un número del oxhidrilo por lo menos igual a cerca de 10 mg/g, ventajoso por lo menos iguales a cerca de 15 mg/g; un igual molecular medio del manganeso de la masa por lo menos a cerca de 1000 g/mol y ventajoso a 2000 g/mol.