This invention provides a method for producing a saponified ethylene-vinyl
acetate copolymer in which visible imperfections (particularly fish eyes)
of the saponified copolymer is inhibited. In this invention, a mixture
solution is prepared by adding water to a methanol solution after
saponifying an ethylene-vinyl acetate copolymer, and insoluble materials
are removed from this mixture solution. Various types of filter or
centrifugal separator are used to remove insoluble materials. It is
preferable that the weight ratio of methanol to water is from 5:5 to 9:1,
the concentration of the saponified copolymer is from 30 to 60 wt %, and
the temperature is from 55 to 80.degree. C. This method is particularly
suitable for producing a saponified ethylene-vinyl acetate copolymer
having an ethylene content of 20 to 70 mol % and a saponification degree
of at least 95 mol %.
Questa invenzione fornisce un metodo per produrre un copolimero saponificato dell'acetato del etilene-vinile in cui le imperfezioni visibili (specialmente occhi dei pesci) del copolimero saponificato è inibita. In questa invenzione, una soluzione della miscela è preparata aggiungendo l'acqua ad una soluzione del metanolo dopo la saponificazione del copolimero dell'acetato del etilene-vinile ed i materiali insolubili sono rimossi da questa soluzione della miscela. I vari tipi di filtro o di separatori centrifughi sono usati per rimuovere i materiali insolubili. È preferibile che il rapporto del peso di metanolo ad acqua è 5:5 - 9:1, la concentrazione del copolimero saponificato è 30 - 60 pesi % e la temperatura proviene da 55 a 80.degree. C. Questo metodo è particolarmente adatto a produrre un copolimero saponificato dell'acetato del etilene-vinile che ha un contenuto dell'etilene di 20 - 70 mol di % e di un grado di saponificazione almeno di 95 mol di %.