The invention involves providing a microstructured fiber having a core
region, a cladding region, and one or more axially oriented elements
(e.g., capillary air holes) in the cladding region. A portion of the
microstructured fiber is then treated, e.g., by heating and stretching the
fiber, such that at least one feature of the fiber microstructure is
modified along the propagation direction, e.g., the outer diameter of the
fiber gets smaller, the axially oriented elements get smaller, or the
axially oriented elements collapse. The treatment is selected to provide a
resultant fiber length that exhibits particular properties, e.g., mode
contraction leading to soliton generation, or mode expansion.
Advantageously, the overall fiber length is designed to readily couple to
a standard transmission fiber, i.e., the core sizes at the ends of the
length are similar to a standard fiber, which allows efficient coupling of
light into the microstructured fiber length.
Вымысел включает обеспечить а microstructured волокно имея зону сердечника, зону плакирования, и one or more осево ориентированные элементы (например, capillary отверстия воздуха) в зоне плакирования. Часть microstructured волокно после этого обработана, например, путем нагревать и протягивать волокно, такое что по крайней мере одна характеристика микроструктуры волокна доработана вдоль направления распространения, например, наружного диаметра волокна получает более малым, осево ориентированные элементы получает более малым, или осево ориентированные элементы рушатся. Обработка выбрана для того чтобы обеспечить возникающую длину волокна exhibits определенные свойства, например, сужение режима водя к поколению soliton, или расширение режима. Выгодн, общая длина волокна конструирована готово для того чтобы соединить к стандартному волокну передачи, т.е., размеры сердечника на концах длины подобны к стандартному волокну, которое позволяет эффективное соединение света в microstructured длина волокна.