A dispersion compensating fiber 1 is placed in the form of a coil or bundle
within a housing 2, and a filling material 3 having a viscosity of 0.01
Pa.multidot.s to 0.6 Pa.multidot.s at normal temperature before curing is
filled in a space around the dispersion compensating fiber 1 within the
housing 2 and then the filling material is cured. As a result, a change of
transmission loss caused by a temperature variation due to heat cycles of
the dispersion compensator can be reduced. A difference in transmission
loss can be further reduced by employing a method of placing the
dispersion compensating fiber in the housing in the form of a loosely
wound bundle and then pouring the filling material, or a method of
applying vibration to the housing, in which the dispersion compensating
fiber is placed, when pouring the filling material.
Eine Zerstreuung ausgleichende Faser 1 wird in Form einer Spule oder eines Bündels innerhalb eines Gehäuses 2 gesetzt, und einem Füllmaterial 3, das eine Viskosität von 0.01 Pa.multidot.s bis 0.6 Pa.multidot.s bei der normalen Temperatur hat, bevor man kuriert, wird ein Raum um die Zerstreuung ausgleichende Faser 1 innerhalb des Gehäuses 2 ausgefüllt und dann wird das Füllmaterial kuriert. Infolgedessen kann eine Änderung des Übertragungsverlustes verursacht durch eine Temperaturveränderung wegen der Hitzezyklen des Zerstreuung Kompensators verringert werden. Ein Unterschied bezüglich des Übertragungsverlustes kann durch das Einsetzen einer Methode die Zerstreuung ausgleichende Faser in das Gehäuse in Form eines Wundbündels lose von legen und das Füllmaterial dann von gießen oder eine Methode des Zutreffens von von Erschütterung auf das Gehäuse weiter verringert werden, in dem die Zerstreuung ausgleichende Faser gelegt wird, wenn das Füllmaterial gegossen wird.