Olefin polymers having a comb-like structure with at least 0.3 long-chain
branches per 1000 carbon atoms are disclosed. Some compositions have a
melt strength of about 5 cN at 190.degree. C., and when made into a film
have a CD shrink of at least 20%. Some compositions described herein
include a high molecular weight fraction and a low molecular weight
fraction wherein the ratio of the molecular weight of the high molecular
weight fraction to the molecular weight of the low molecular weight
fraction is greater than about 1.3.