A method of making an electrolytic cell in which an electrolyte layer of
an intermediate sintered form is coated with a pre-coat layer containing
electrically non-conductive particles of less than about one-tenth of a
micron in size to fill in defects existing within the electrolyte layer.
The pre-coat layer is removed so that the electrically non-conductive
particles remain within the defects of the electrolyte layer. The cathode
layer is then applied to the electrolyte layer with the electrically
non-conductive particles in place within the defects. The intermediate
sintered form is fired with the applied cathode layer to produce the
electrolytic cell.