The present invention is characterized in having the structure which can
reduce reflection ratio of exterior light when the device is not
operating, that is, when light is not emitted from the device. To this
end, the structural elements formed on the non-emitting areas are formed
with dark color black matrix material. To have the structure, the present
organic electroluminescent device comprises indium-tin-oxide (ITO) layers
formed on a glass substrate; insulating layers formed on non-emitting
area of the ITO layers, each insulating layer being formed with dark
colored material; a plurality of walls formed on the insulating layers;
and organic electroluminescence layers and metal layers formed
sequentially on the entire structure including the walls, the organic
electroluminescence layers and metal layers being separated from adjacent
organic electroluminescence layers and metal layers by the walls. Each
insulating layer is consisted of a black matrix film formed on the ITO
layer and an insulating film formed on the black matrix film in the shape
of wrapping the black matrix material layer. On the contrary, each
insulating layer formed below the wall is consisted of an insulating
layer formed on the ITO layer and a black matrix film formed on the
insulating film. Also, in the present organic electroluminescent device,
the walls can be formed with back matrix material.