Provided is a manufacturing method of high purity oxide powder including
the steps of subjecting a raw material such as Zn-containing scrap to
acid leaching or electrolytic extraction, thereafter performing solvent
extraction and activated carbon treatment thereto in order to remove
impurities, neutralizing the resultant solution freed of impurities with
an alkaline solution to obtain zinc hydroxide, and firing the zinc
hydroxide to obtain zinc oxide. Provided are high purity zinc oxide
efficiently freed of impurities, in particular C, Cl, S and Pb
impurities, at low cost and the manufacturing method thereof; a target
manufactured by firing the high purity zinc oxide; and a high purity zinc
oxide thin film obtained by the sputtering the target.