According to the method, the transversal wire or rebar to be formed (1) and the longitudinal wires or rebars or other material of prismatic cross section (2), (3) are fed to the main forming and welding machine subsystem, in a stepwise manner, at the appropriate distance each time, through a driving mechanism (22-30). At this location, the transversal wire (1) is cut and then formed upon the action of a press (36). Welding of the formed transversal frame with one of the two longitudinal wires is performed while the formed transversal wire is still restrained by the action of the press (38) at the formation location. Welding with the second longitudinal wire is performed at the next production step, simultaneously with the welding of the next transversal frame with the first longitudinal wire, at the formation location. After the welding action, the transversal frame is released by the press and the forming tools (37-39), and the next production step is initiated. The product is made in a continuous shape and is cut at the proper lengths, by a cutter (45).

 
Web www.patentalert.com

< Energetic composite materials containing inorganic particle network, and articles of manufacture and methods regarding the same

> Perforation gun system for sealing perforation holes

> Electro-magnetically operated rotating projectile loader

~ 00554