A method for dehydrating a monolithic bone intended for implantation is
provided. The method serves to conserve at least one of the biomechanical
properties of the bone during the dehydration of the bone and its
subsequent packaging. Also provided is a monolithic bone for implantation
and a method of using the bone for the repair of damaged bone.